One navy wool sweater can need four different fastness tests before anyone agrees it is safe to sell. Wash, rubbing, perspiration and light each simulate a different contact, and a garment that passes one can still stain a white shirt or fade on a rail. Apparel colorfastness test selection is the job of matching the test to the exposure.
Most buyers inherit a list of tests from a previous program and keep running it. That is how a summer cotton tee ends up with a light fastness report nobody reads and no wet crocking result for a dark indigo print that will sit against a pale bag strap.
Apparel colorfastness test selection: the short answer
Apparel colorfastness test selection should follow three variables: how the garment is washed, what it touches when worn, and how dark or saturated the shade is. Wash fastness covers laundering, rubbing covers dry and wet contact, perspiration covers skin contact, and light covers display. Test the exposures the product will actually meet.
That is the logic. The rest of this page sets out what each test measures, how it is run, and how to read the report when it comes back.
Four tests, one garment
The four core tests answer four different questions. Wash fastness asks whether the dye stays put in water and detergent, and whether it migrates onto other fabrics in the same load. Rubbing asks whether colour transfers by contact, dry or wet. Perspiration asks whether sweat changes the shade or stains a neighbouring fabric. Light asks whether the shade survives exposure to daylight.
A garment does not need all four equally. A black wool coat needs rubbing and light, because it will be worn against pale shirts and displayed in a window. A white cotton tee needs wash and perspiration, because the visible failure is yellowing and greying rather than transfer.
The mistake is choosing by habit rather than by exposure. Ask what the customer will do to the garment in the first month, and the list writes itself.
What each test actually does
Wash fastness is run on a specimen sewn to a multi-fibre strip, so the same wash shows both change in the sample and staining of adjacent fabrics. The strip carries wool, cotton, nylon, polyester, acrylic and acetate, and the report grades each one separately. Conditions vary by method and by the care label, and the temperature, detergent and mechanical action all change the result.
Rubbing, usually called crocking, is run dry and wet. A white cloth is rubbed against the specimen under controlled pressure, and the cloth is graded for staining. Wet crocking matters most on dark, saturated shades and on prints, because water releases surface dye that dry rubbing never touches.
Perspiration testing uses two solutions, one acid and one alkaline, to represent the range of human sweat. The specimen is soaked, pressed against adjacent fabric, dried, and graded for change and staining. It is the test that catches reactive dyes that were not washed off properly after dyeing.
Light fastness exposes the specimen to a controlled light source and compares the faded area with an unexposed control. It matters for shop windows, outdoor wear and pale shades that yellow rather than fade to a visibly different tone.
| Test | What it simulates | What the report grades | Most relevant to |
|---|---|---|---|
| Wash | Laundering with detergent and mechanical action | Change in shade and staining of a multi-fibre strip | Anything machine washable |
| Rubbing (dry) | Contact with another surface | Staining of a white cloth | Dark shades, prints, trims |
| Rubbing (wet) | Contact while damp, including sweat and rain | Staining of a white cloth | Indigo, saturated colours, activewear |
| Perspiration | Acid and alkaline sweat against skin or lining | Change in shade and staining | Collars, cuffs, linings, pale shades |
| Light | Daylight or shop-window exposure | Change in shade against a control | Display pieces, outdoor wear |
Read the fourth column as a starting point, not a rule. A pale garment can still fail wet crocking if a dark trim bleeds onto it, and a dark garment can fail perspiration if the dye is unstable at skin pH.
Choosing by use, then by shade
Start with the care label the garment will carry. If it says machine wash warm, wash fastness is not optional. If it says hand wash cold, the wash test still applies but the conditions change, and the report has to say which conditions were used or the number cannot be compared with the next program.
Then look at the shade. Deep blacks, navies, reds and indigos are the shades most likely to crock, because the dye loading is high and the surface carries unfixed dye. Pale shades fail differently: they yellow, grey or pick up colour from whatever they are washed with, which is a staining question rather than a fading one.
Finally, look at the construction. A garment with a contrast lining, a dark trim on a pale body or a printed panel against a white ground has an internal transfer risk that a single-fabric test will not show. In those cases the test specimen should include both materials sewn together.
Prints deserve their own line in the spec. A plastisol print covers the fabric and hides the base shade, while a water-based or discharge print sits in the yarn and behaves like a dye. If the print is the visible surface, test the print rather than the fabric beneath it, and include a wash and a wet rub.

Reading the report
Fastness results are reported on grey scales, one for change in shade and one for staining, and the two are not interchangeable. A result of 4–5 for change and 3 for staining describes a garment that keeps its own colour but marks what it touches, which is exactly the failure a customer notices on a white sofa.
The multi-fibre strip produces a row of staining grades, one per fibre. Read the row rather than the average, because the fibre that stains worst tells you what the garment will damage: wool staining badly is a problem for coats and knitwear layered together, acetate staining badly is a problem for linings.
Conditioning and assessor judgment both affect the number. Two laboratories grading the same specimen can differ by half a grade, which is why a requirement should state the scale and the method, and why a single grade without either is not a specification.

Writing the requirement so it can be checked
A testable requirement names the method, the conditions, the scale and the acceptance level. It also states the consequence: reject, re-test, or accept with a deviation. Without that, the report arrives and the argument starts.
Ask the laboratory to confirm the current edition of each method before the spec is signed. Methods are revised, and a program that has run for years on an old edition may be comparing results that are no longer equivalent.
Keep the requirement stable across seasons, and change it deliberately when the product changes. A new dye lot, a new fabric supplier or a new wash process can move a result without anything in the design changing.
FAQ
Do we need every fastness test on every style?
No. Choose by the care label and the way the garment is worn. Wash and rubbing cover most apparel, perspiration matters for anything against skin, and light matters for display and outdoor pieces. A test nobody reads costs money and adds nothing.
What is the difference between dry and wet crocking?
Dry crocking rubs a dry cloth against the fabric and catches surface pigment. Wet crocking does the same with a damp cloth and catches dye that water releases. Dark and saturated shades often pass dry and fail wet, which is why both are run.
Can we test the garment instead of the fabric?
Yes, and for garments with contrast trims or linings it is the more honest test. A fabric test describes the material; a garment test describes what the customer actually handles, including seams and joins where two dyes meet.
What do the grey scale numbers mean?
They describe the size of the visible difference against a standard, from 1 for a large change to 5 for none. The scale is not a percentage and does not translate into a wash count. The acceptance level for your market should come from the brand or the retailer’s standard.
Agreeing the list before the first bulk
Four tests, chosen by exposure, written with method and acceptance level, will catch most of what a customer would otherwise discover. The list is short enough to fit on a page and specific enough for a laboratory to price without a meeting.
One more habit pays off: keep the last few reports for the same shade beside the approved standard. When a customer returns a garment that has bled, the comparison tells you whether the dye changed, the wash process changed, or the complaint is about something else entirely.
Send the care label and the shade range with the tech pack, and state which tests are required and which are optional. Our manufacturing services page covers how testing is scheduled around sampling, and the questions buyers ask before sampling include the ones that surface a fastness risk early. Sampling is 7–12 days after fabric and tech pack approval, with bulk typically 20–35 days after sample approval.
Sources: Intertek, Control Union, Higg, OEKO-TEX Standard 100, EU Regulation 1007/2011 on textile fibre names and US CBP informed compliance publications.
Working on a knitwear project?
Let’s talk yarn, gauge and timing.
Send a reference or tech pack and we will come back with a practical development route.